Structural Assessment

Structural Assessment

Inspection and assessment of old buildings or structures follow engineering principles and a standard process to ensure safety and extend service life. The work is generally divided into 4 main steps:

1. Preliminary Inspection
(Visual Inspection)

The first step is a walk-through visual survey with basic inspection tools to assess the general condition of the building or structure.

  • Crack survey: classifying cracks, such as thermal cracks, structural cracks caused by overloading, or cracks caused by differential settlement.
  • Concrete surface failure: checking for spalling that exposes the reinforcing steel.
  • Alignment & Plumb check: checking whether columns or beams show deflection, or whether the building is tilting.
  • Environmental assessment: checking moisture, standing water or chemicals that may corrode the structure.
Visual Inspection 1

2. In-depth Inspection
(Non-Destructive Testing - NDT)

Special testing equipment is used without damaging the structure, to evaluate concrete strength and inspect the internal condition of the structure.

  • Rebound Hammer Test (Schmidt Hammer)
    An impact hammer is used to estimate the compressive strength of the concrete.
  • Ferroscan
    Electromagnetic scanning to locate the reinforcing steel and measure its size and concrete cover (Covering) without drilling or chipping the concrete.
  • Ultrasonic Pulse Velocity (UPV)
    High-frequency sound waves are passed through the concrete to check its density and find voids or internal cracks.
Non-Destructive Testing (NDT)

3. Partially Destructive Testing
(Partially Destructive Testing)

Where high accuracy is needed for detailed engineering calculations, samples must be taken from the actual structure.

  • Concrete Core Drilling
    Concrete cores are cut from the structure and tested in a compression machine in the laboratory (Lab) to find the true compressive strength of the concrete.
  • Carbonation Test
    Testing the pH of the concrete to assess the loss of alkalinity and analyse the risk of corrosion of the reinforcing steel.
  • Chloride Content Test
    Concrete powder is extracted and tested for chloride content — the main cause of rusting reinforcement, which expands and cracks the concrete.
Partially Destructive Testing

4. Engineering Analysis and Evaluation
(Engineering Analysis & Assessment)

Once all the raw data and test results are available, structural engineers use them to evaluate the building as a whole.

  • As-Built Drawing
    Preparing drawings of the structure as it currently stands, for old buildings whose original drawings no longer exist.
  • Structural Software Modeling
    The measured material strengths are entered into structural analysis software to check whether the building can still carry its loads (Load Carrying Capacity) to current standards.
  • Summary and Recommendations (Reporting)
    A report summarising the building's condition, classifying the level of damage and the corrective approach, for example:
    • Normal / general maintenance level
      Paint to seal fine (map) cracks
    • Structural repair level (Repair)
      Chip out the concrete, apply rust inhibitor, then patch with Non-shrink Grout
    • Strengthening level (Retrofitting/Strengthening)
      e.g. Carbon Fiber (CFRP) wrapping, column section enlargement (Section Enlargement) or steel jacketing (Steel Jacketing)
Engineers presenting structural analysis results with a 3D model

Other Products & Services